| Sign In | Join Free | My benadorassociates.com | 
 | 
Model Number : LR-300C
Place of Origin : China
Brand Name : Lonroy
MOQ : 1
Price : Negotaible
Packaging Details : Wooden package
Delivery Time : 5-8 work days
Supply Ability : 200
Temperature range : room temperature ~550ºC
Heating rate : 0.1 ~ 80ºC/min
DSC range : 0 ~ ±600mW
Data interface : standard USB interface
Power supply : AC220V/50Hz
Certification : ISO ASTM CE
Payment Terms : L/C,D/A,D/P,T/T,Western Union
ISO 11357 Calorimeter DSC Differential Scanning Calorimeter Differential Scanning Calorimetry Test
1. Product Introduction
LR-300 is the company launched DSC series of products with the highest accuracy of one, the sensor is the use of imported material E-couple, high precision, high sensitivity, good repeatability, signal acquisition circuit shielding protection, strong anti-interference, baseline stability and repeatability is very high.
LR-300 differential scanning calorimeter, can be glass transition temperature, phase transition temperature, melting point, enthalpy value, curing temperature and product stability, oxidation induction period and other tests. It is qualified for the research of pipe, polymer, chemical, food, medical and other fields, and serves universities, enterprises, third-party measurement and quality inspection units, with a wide range of applications to meet the testing needs of various industries.
2. Technical features
1. Industrial grade 7 inch touch screen, display rich information
2. New furnace body structure, better baseline, higher accuracy. Heating adopts indirect conduction mode, high uniformity and stability, reduce pulse radiation, better than the traditional heating mode.
3.USB communication interface, strong commonality, reliable communication without interruption, support self-recovery connection function.
4. Automatic switching of two air flow, fast switching speed, short stability time. At the same time, a protective gas input is added.
5. Software is simple and easy to operate.
6. Ultra-high sensitivity, accuracy, 0.001 MW, 0.001ºC
7. Exquisite technical indicators, superior performance, cost-effective, widely used.
3. Technical parameters
| Temperature range | room temperature ~550ºC | 
| temperature resolution | 0.001ºC | 
| temperature fluctuation | ±0.001ºC | 
| Temperature repeatability | ±0.01ºC | 
| Heating rate | 0.1 ~ 80ºC/min | 
| Constant temperature time | program setting ≤24h | 
| Temperature control mode | heating, constant temperature, cooling (automatic program control) | 
| DSC range | 0 ~ ±600mW | 
| DSC resolution | 0.01uW | 
| DSC sensitivity | 0.001mW | 
| Power supply | AC220V/50Hz or customized | 
| Atmosphere control gas | nitrogen, oxygen (program setting/automatic switch) | 
| Gas flow | 0-300ml /min | 
| gas pressure | 0.2mpa | 
| Display mode | 24bit color, 7 inch LCD touch screen display | 
| Data interface | standard USB interface | 
| Parameter standard | equipped with standard material (indium, tin), users can adjust the temperature by themselves | 
| The instrument has multiple groups of thermocouples, one group to measure sample temperature, one group to measure furnace body temperature, and one group to measure internal environment temperature | |
| Cooling device | air cooling device (optional semiconductor & LT; - 40 ~ 550 ºC & gt; Liquid nitrogen refrigeration < - 150 ~ 550 ºC & gt;) | 
|   | 
| AC220V 50Hz DSC Differential Scanning Calorimeter Differential Scanning Calorimetry Test Images | 
 ASTM E1354 ISO 5660 BS 476 Cone Calorimeter Analyzer Cone Calorimetry Tester
                                                                                    
                        
                        
                        
                                                            ASTM E1354 ISO 5660 BS 476 Cone Calorimeter Analyzer Cone Calorimetry Tester
                                                    
                        
                     Fully Automatic Oxygen Bomb Calorimeter DM3300 Certification Includes Calibratio
                                                                                    
                        
                        
                        
                                                            Fully Automatic Oxygen Bomb Calorimeter DM3300 Certification Includes Calibratio
                                                    
                        
                     ISO 5660 ASTM E1354 BS 476 Cone Calorimeter Tester Equip with Imported Siemens
                                                                                    
                        
                        
                        
                                                            ISO 5660 ASTM E1354 BS 476 Cone Calorimeter Tester Equip with Imported Siemens
                                                    
                        
                     BS 476 ASTM E1354 ISO 5660 Cone Calorimeter Testing Device Cone Calorimetry
                                                                                    
                        
                        
                        
                                                            BS 476 ASTM E1354 ISO 5660 Cone Calorimeter Testing Device Cone Calorimetry
                                                    
                        
                     LRR-3C Automatic Temperature Specific Heat Capacity Tester With Adiabatic Method
                                                                                    
                        
                        
                        
                                                            LRR-3C Automatic Temperature Specific Heat Capacity Tester With Adiabatic Method
                                                    
                        
                     LR-SPY Ceramic Tile Wet Expansion Tester 220V 5kW Wet Expansion Machine
                                                                                    
                        
                        
                        
                                                            LR-SPY Ceramic Tile Wet Expansion Tester 220V 5kW Wet Expansion Machine
                                                    
                        
                     LRPL-II ASTM C518 Automatic Thermal Resistance Tester Plate Heat Flux Meter
                                                                                    
                        
                        
                        
                                                            LRPL-II ASTM C518 Automatic Thermal Resistance Tester Plate Heat Flux Meter
                                                    
                        
                     3kW Thermal Conductivity Testing Machine Measurement Heat Conduction Sensor
                                                                                    
                        
                        
                        
                                                            3kW Thermal Conductivity Testing Machine Measurement Heat Conduction Sensor
                                                    
                        
                     Desktop Thermal Conductivity Testing Equipment Plate Heat Flux Meter Method
                                                                                    
                        
                        
                        
                                                            Desktop Thermal Conductivity Testing Equipment Plate Heat Flux Meter Method
                                                    
                        
                     LRPY-300 10N Thermal Analysis Instrument Plastic Expansion Meter
                                                                                    
                        
                        
                        
                                                            LRPY-300 10N Thermal Analysis Instrument Plastic Expansion Meter